Polipol™ 305 - Plasto Fiberglass

Transkript

Polipol™ 305 - Plasto Fiberglass

                                    

Benzer belgeler

Polipol™ 354

Polipol™ 354 temperatures between 5°C and 20°C. Shelf life is reduced at higher temperatures. The shelf life of styrene containing unsaturated polyesters will be significantly reduced when exposed to light. Sto...

Detaylı

Polipol™ 3401-TAB - Plasto Fiberglass

Polipol™ 3401-TAB - Plasto Fiberglass Polipol 3401-TAB contains a blue colored Mek-p indicator, its color disappears after a couple of minutes when it’s mixed with Mek-p. As known the addition of Mek-p to resin is done automatically at...

Detaylı

Polipol™ 391

Polipol™ 391 temperatures between 5°C and 20°C. Shelf life is reduced at higher temperatures. The shelf life of styrene containing unsaturated polyesters will be significantly reduced when exposed to light. Sto...

Detaylı

Polives 702

Polives 702 temperatures between 5°C and 20°C. Shelf life is reduced at higher temperatures. The shelf life of styrene containing unsaturated polyesters will be significantly reduced when exposed to light. Sto...

Detaylı

Polives™ 701

Polives™ 701 .1. The product should be stored in a dark and dry place at temperatures between 5°C and 20°C. Shelf life is reduced at higher temperatures. The shelf life of styrene containing unsaturated polyest...

Detaylı

Polipol™ 320-TA - Omnis Kompozit

Polipol™ 320-TA - Omnis Kompozit .1. The product should be stored in a dark and dry place at temperatures between 5°C and 20°C. Shelf life is reduced at higher temperatures. The shelf life of styrene containing unsaturated polyest...

Detaylı

Polijel™ 211 - Omnis Kompozit

Polijel™ 211 - Omnis Kompozit temperatures between 5°C and 20°C. Shelf life is reduced at higher temperatures. The shelf life of styrene containing unsaturated polyesters will be significantly reduced when exposed to light. Sto...

Detaylı

Polijel™ 210 TOPCOAT 933 WHITE

Polijel™ 210 TOPCOAT 933 WHITE temperatures between 5°C and 20°C. Shelf life is reduced at higher temperatures. The shelf life of styrene containing unsaturated polyesters will be significantly reduced when exposed to light. Sto...

Detaylı

Fleksotix - Omnis Kompozit

Fleksotix - Omnis Kompozit significant reduction in gel-time. So; for applications where shorter gel-times are needed, an addition of 0,1% Cobalt solution (6% concentration) is advised, which will give about 10 minutes reduc...

Detaylı

VEtix

VEtix temperatures between 5°C and 20°C. Shelf life is reduced at higher temperatures. The shelf life of styrene containing unsaturated polyesters will be significantly reduced when exposed to light. Sto...

Detaylı

poliya selection guide V11.cdr

poliya selection guide V11.cdr El Yatırması Hand lay-up Elyaf Püskürtme Spray-up Fitil Sarma Filament Winding Sürekli Çekme Continuous Laminating Döküm Casting RTM Resin Transfer Moulding Soğuk Pres Cold Pres Sıcak Pres (SMC-BMC...

Detaylı

Mold Making Guide.cdr

Mold Making Guide.cdr document and the user faults. Also we highly recommend you to make tests in your own working conditions before using products on your production. Poliya can change any data provided on this documen...

Detaylı

kimyasal dayanım kılavuzu chemıcal resıstance

kimyasal dayanım kılavuzu chemıcal resıstance The information provied on this data sheet is prepared with longterm laboratory tests and our own experiences. The information is given with goodwill to act as a guide but not as reference also Pol...

Detaylı